12th International Conference on Zinc & Zinc Alloy Coated Steel Sheet - GALVATECH 2021

from Sunday, 20 June 2021 (08:00) to Thursday, 24 June 2021 (18:00)
Virtuel Conference

        : Sessions
    /     : Talks
        : Breaks
21 Jun 2021
22 Jun 2021
23 Jun 2021
AM
08:30
Opening (until 08:40) (Room A)
08:40
1 - Plenary Talk 1 - Europe (until 09:00) (Room A)
08:40 EUROPE: TOMORROW JUST AROUND THE CORNER? - Dr Thomas Koll   (Room A)
Paper
09:00
2 - Plenary Talk 2 - Korea (until 09:20) (Room A)
09:00 RECENT PROGRESS OF ZINC AN ZINC ALLOY COATED STEEL SHEETS IN KOREA - Jong_Sang Kim (POSCO)   (Room A)
Paper
09:20
3 - Plenary Talk 3 - Japan (until 09:40) (Room A)
09:20 RECENT DEVELOPMENTS AND OUTLOOK ON ZINC AND ZINC ALLOY COATED STEEL SHEETS IN JAPAN - Nobuhiro Fujita (Nippon Steel)   (Room A)
Paper
09:40
4 - Plenary Talk 4 -USA (until 10:00) (Room A)
09:40 NORTH AMERICAN DEVELOPMENTS AND OPPORTUNITIES FOR GALVANIZED STEEL SHEET - Dr Frank Erik Goodwin (International Zinc Association)   (Room A)
Paper
10:00
5 - Plenary Talk 5 - China (until 10:20) (Room A)
10:00 DEVELOPMENT OF ZINC AND ZINC-ALLOY COATED STEEL SHEET IN CHINA - Qifu Zhang (China Iron & Steel Res. Institute Group)   (Room A)
Paper
10:20 --- Break ---
10:50
Automotive Applications - ZnAlMg Coatings -Mr Friedhelm Macherey (thyssenkrupp Steel Europe AG) (until 12:30) (Room A)
10:50 Current use and future outlook of coated sheet steel at Volvo Cars - Richard Johansson (VOLVO CAR CORPORATION)   (Room A)
11:10 INVESTIGATION OF HOT-DIP ZnMgAl COATINGS FOR AUTOMOTIVE APPLICATIONS - Tae Chul Kim (POSCO)   (Room A)
Paper
11:50 ANTI-CORROSION PERFORMANCE OF ZnMg AND ZnMgAl-COATED STEELS FOR AUTOMOTIVE APPLICATIONS - Yun Ha Yoo (POSCO)   (Room A)
Paper
10:50
Coating Microstructure Analysis and Steel/Coating Surface Reactivity -Dr Anirban Chakraborty (ArcelorMittal) (until 12:30) (Room C)
10:50 SCANNING KELVIN PROBE TECHNIQUES FOR THE INVESTIGATION OF CORROSION, HYDROGEN UPTAKE AND PERMEATION PROPERTIES OF ZINC ALLOY COATINGS ON STEEL - Michael Rohwerder (Max-Planck-Institut für Eisenforschung GmbH)   (Room C)
Paper
11:10 ON GRAIN BOUNDARY TOPOGRAPHY AND SURFACE REACTIVITY DURING HOT-DIP GALVANISING - Nils Köpper (Salzgitter Mannesmann Forschung GmbH)   (Room C)
Paper
11:30 DENDRITIC MORPHOLOGIES OF HOT-DIP GALVANIZED Zn-0.2 WT.% Al COATINGS: EXISTENCE OF THIRD PREFERRED GROWTH DIRECTIONS - Joo-Youl Huh (Korea University)   (Room C)
Paper
11:50 MICROSTRUCTURE AND TEXTURE ANALYSIS OF A NEAR-EUTECTIC Zn-Al COATING DEPOSITED ON STEEL BY HOT-DIP GALVANIZING - Houssem Eddine Chaieb (Mines ParisTech)   (Room C)
Paper
12:10 SEGREGATION MECHANISM OF Al-BASED OXIDES ON Zn-0.2MASS%Al HOT-DIP GALVANIZED STEEL SHEETS - Katsuya Hoshino (JFE Steel Corporation)   (Room C)
Paper
10:50
Furnace I - Temperature Control Challenges - Omar Garcia-Rincon (TERNIUM Mexico SA de CV) Sergey Yashchuck (Severstal) (until 12:30) (Room B)
11:10 NONLINEAR MODEL PREDICTIVE TEMPERATURE CONTROL OF A COMBINED DIRECT- AND INDIRECT-FIRED STRIP ANNEALING FURNACE - Martin Niederer (Austrian Institute of Technology / Center for Vision, Automation & Control)   (Room B)
Paper
11:30 EFFECT OF ANNEALING ATMOSPHERE AND STEEL ALLOY COMPONENTS ON SURFACE TOPOGRAPHY AND RADIATIVE PROPERTIES OF ADVANCED HIGH STRENGTH STEEL STRIP DURING CONTINUOUS GALVANIZING - Kaihsiang Lin (University of Waterloo)   (Room B)
Paper
11:50 INCREASING LIFETIME OF METALLIC RADIANT TUBES IN VERTICAL GALVANIZING LINES - Nico Schmitz (Department for Industrial Furnaces and Heat Engineering / RWTH Aachen University)   (Room B)
Paper
12:10 APPLICATION OF A PHYSICS-BASED EMPIRICAL MODEL FOR ESTIMATION OF RADIANT TUBE TEMPERATURES IN A GALVANIZING LINE - Alexander Reimann (Department for Industrial Furnaces and Heat Engineering (RWTH Aachen University))   (Room B)
Paper
08:30
Industrial Status of Galvanizing Production Technology -Mr Sho Katsura (KOBE STEEL, LTD.) Prof. Joseph McDermid (McMaster University) (until 10:10) (Room B)
08:30 HOT-DIP GALVANIZING LINES - CHALLENGES AND SOLUTIONS FOR THE INDUSTRIAL PRODUCTION OF COATED 3rd GEN AUTOMOTIVE STEELS - Thomas Daube (SMS group Gmbh) Lutz Kümmel (SMS group Gmbh) Holger Behrens (SMS group GmbH)   (Room B)
Paper
08:50 FIVES’ EYERON™, ALL-IN-ONE QUALITY MANAGEMENT SOFTWARE - Maxime Monnoyer (Fives KEODS)   (Room B)
Paper
09:10 EFFICIENT AND EFFECTIVE OPERATION OF A HOT DIP GALVANIZING LINE - Massimiliano Svetina (Danieli)   (Room B)
Paper
09:30 THROUGH-PROCESS OPTIMIZATION (TPO) - A MODERN APPROACH TO RAPID PRODUCT DEVELOPMENT - Sergey Bragin (Primetals)   (Room B)
Paper
09:50 NEWEST GENERATION OF METRIS ADVANCED FURNACE CONTROL FULFILS HIGHEST QUALITY DEMANDS - Andreas Argårds (SSAB) Martin Fein (Andritz AG)   (Room B)
08:30
LME of Resistance Spot Welded Coated Steels: Assessments - Sanna Järn (SSAB) Dr Sven Erik Hörnström (SSAB EMEA AB) (until 10:10) (Room A)
08:30 APPLICATION-ORIENTED AVOIDANCE OF LIQUID METAL EMBRITTLEMENT DURING RESISTANCE SPOT WELDING OF ZINC-COATED ADVANCED HIGH STRENGHT STEELS - Mr Christoph Böhne (Universität Paderborn - LWF)   (Room A)
08:50 EVALUATION OF INITIATION AND PROPAGATION OF LME CRACKS ON THE GALVANIZED 3G-AHSS USING INTERRUPTED RESISTANCE SPOT-WELDING METHOD - Anirban Chakraborty (ArcelorMittal)   (Room A)
Paper
09:10 COMPARATIVE ASSESSMENT OF GI AND GA COATED AHSS LME SENSITIVITY DURING SPOT WELDING - Mr Jean-Michel Mataigne   (Room A)
Paper
09:30 NUMERICAL MODEL FOR PREDICTING LIQUID METAL CRACKING DURING RESISTANCE SPOT WELDING OF ADVANCED HIGH STRENGTH STEELS - Konstantin Manuel Prabitz (Materials Center Leoben Forschung GmbH)   (Room A)
Paper
08:30
Solidification and Formation of Hot Dip Galvanized Coatings -Prof. Dave Penney Daniel Liu (until 10:10) (Room C)
08:30 INFLUENCE OF SURFACE ROUGHNESS OF FULL HARD STEEL ON SPANGLE OF GALVANIZED STEEL AND ACTUAL APPLICATION RESULTS - TAE JUN PARK (Hyundai-steel)   (Room C)
Paper
08:50 SPANGLE NUCLEATION AND REFINEMENT THEORY IN 55%Al-Zn COATED STEEL - Nega Setargew (BlueScope Steel Innovation Labs)   (Room C)
Paper
09:10 PERITECTIC STRUCTURE EVOLUTION IN HOT-DIP Zn-Al ALLOY COATINGS - Takuya Mitsunobu (Nippon Steel Corporation)   (Room C)
Paper
09:30 RAPID DESIGN OF NEW Zn-Mg-Al-Sn COATINGS WITH LOW MELTING POINT FOR AUTOMOTIVE SHEET APPLICATIONS VIA MACHINE LEARNING - Rohit Bardapurkar (Colorado School of Mines)   (Room C)
Paper
10:10 --- Break ---
10:40
LME of Resistance Spot Welded Coated Steels: Moving Toward Solutions - Kyle Daun Jonas Staudte (ArcelorMittal Maizières) (until 12:20) (Room A)
11:00 EFFECT OF Zn-COATING PROCESS ON LIQUID METAL EMBRITTLEMENT OF TRIP STEEL - Doyub Kim (Graduate Institute of Ferrous Technology, POSTECH, South Korea)   (Room A)
Paper
11:20 QUANTITATIVE ASSESSMENT OF THE INFLUENCE OF STARTING MICROSTRUCTURE ON THE LIQUID METAL EMBRITTLEMENT SUSCEPTIBILITY OF 3rd GENERATION ADVANCED HIGH STRENGTH STEELS - Diptak Bhattacharya (Graduate Research Assistant, Advanced Steel Processing and Product Research Center (ASPPRC), Colorado School of Mines)   (Room A)
Paper
10:40
On-line Measurements - Cleanliness, Austenite Fraction and Coating Defects -Ms Frances Bleich (ArcelorMittal USA) (until 12:20) (Room B)
10:40 CLEANLINESS MEASUREMENT BY INNOVATIVE LIBS METHOD - Thomas Gossuin (CRMGroup)   (Room B)
Paper
11:00 PRODUCER EXPERIENCES AND ADVANCEMENTS WITH AN ONLINE, NON-CONTACT SURFACE CLEANLINESS MONITOR - Eric Almquist (Star Tool & Die Works)   (Room B)
Paper
11:20 NEW APPROACH FOR ONLINE AUSTENITE FRACTION MEASUREMENT FORMED DURING CONTINUOUS ANNEALING PROCESS. PART I: MEASURE ON HIGH STRENGTH MICROALLOYED STEEL GRADES - Alessandro Ferraiuolo (Marcegaglia Ravenna)   (Room B)
Paper
11:40 IN-LINE CHARACTERISATION OF THE AUSTENITE LEVEL TO ENSURE THE MECHANICAL PROPERTIES ALONG THE COIL - Olivier Herbiet (CRM GROUP)   (Room B)
Paper
12:00 SIAS® 4.0 - THE NEXT GENERATION OF AUTOMATIC SURFACE INSPECTION SYSTEM USING CONVOLUTIONAL NEURON NETWORK FOR DETECTION AND CLASSIFICATION OF SURFACE DEFECTS - Yvon Fontaine (Clecim S.A.S.)   (Room B)
Paper
10:40
PHS-AlSi & PHS-ZnFe: Controlling Surface Properties - Weiping Sun Dr Paul Janavicius Janavicius (AK Steel Research and Innovation) (until 12:20) (Room C)
10:40 NEW COATING FOR PRESS HARDENED STEELS: AlSiZnMg - Tiago Machado (ArcelorMittal)   (Room C)
Paper
11:00 ON THE REDUCTION OF TEMPERATURE GRADIENTS WITHIN AlSi-COATED BLANKS WITH NON-CONSTANT SHEET THICKNESS FOR HOT PRESS FORMING APPLICATION - Friedrich Luther (Salzgitter Mannesmann Forschung GmbH)   (Room C)
Paper
11:20 INFLUENCE OF OXIDE COMPOSITION AND SHOT BLASTING PARAMETERS ON SURFACE RESISTANCE OF GALVANIZED PRESS HARDENED STEELS - Ernst Dietmar Schachinger (voestalpine Stahl GmbH)   (Room C)
Paper
11:40 NANOSCALE STRUCTURE AND COMPOSITIONAL ANALYSIS OF SURFACE OXIDES ON HOT-DIP GALVANIZED PRESS-HARDENED STEEL - Wolfgang Gaderbauer (Christian Doppler Laboratory for Nanoscale Phase Transformations, Center for Surface and Nanoanalytics, Johannes Kepler University Linz)   (Room C)
Paper
08:30
Fundamentals on Surface Oxidation and Wettability -Dr GUANGRUI JIANG (Shougang Group) Mr Eduardo Silva (United States Steel Corporation) (until 10:10) (Room A)
08:30 IMPROVEMENT OF WETTABILITY BETWEEN STEEL AND LIQUID Zn-Al ALLOY BY FORCED WETTING - Marie-Laurence Giorgi (CentraleSupélec)   (Room A)
Paper
08:50 MITIGATION OF THE ADVERSE EFFECTS OF INCREASING Si CONTENT IN A CMnSi ADVANCED HIGH STRENGTH STEEL VIA CONTROLLING ANNEALING ATMOSPHERE pO2 AND MINOR Sn ADDITION DURING CONTINUOUS GALVANIZING - Ghazal Seyed Mousavi (McMaster Steel Research Center, McMaster University, Hamilton, Canada)   (Room A)
Paper
09:10 AHSS SURFACE OXIDE PHASE FORMATION DURING ANNEALING AND PREDICTING THEIR TYPE USING GIBBS ENERGY MINIMIZATION (GEM) THERMODYNAMIC PRINCIPLE - Daniel Liu (Teck Metals Limited) Venu Krishnardula (ArcelorMittal Global R&D)   (Room A)
Paper
09:30 REACTIVE WETTING OF MEDIUM-Mn ADVANCED HIGH-STRENGTH STEELS BY A Zn-Al-Mg BATH - Maedeh Pourmajidian (Steel Research Centre, McMaster University)   (Room A)
08:30
Origins of Hydrogen Embrittlement -Dr Louis Bordignon (CRM group) Mr Takuya Mitsunobu (until 10:10) (Room C)
08:30 EFFECT OF ANNEALING ATMOSPHERE ON HYDROGEN EMBRITTLEMENT OF ADVANCE HIGH STRENTH STEEL - JoungHyun La (Hyundai steel)   (Room C)
Paper
08:50 INFLUENCE OF Zn-BASED COATING ALLOYS ON HYDROGEN DIFFUSION AND CORROSION RESISTANCE IN A DP STEEL - Mélodie MANDY (CRM group)   (Room C)
Paper
09:10 CHARACTERIZATION OF RESIDUAL STRESSES AT SHEARED, MILLED AND LASER CUT EDGES IN MARTENSITIC STEELS - Sven Erik Hörnström (SSAB EMEA AB)   (Room C)
Paper
09:30 INVESTIGATIONS ON CORROSION BEHAVIOR AND HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY OF GALVANIZED DUAL-PHASE STEEL - Ines Traxler (CEST Competence Center for Electrochemical Surface Technology, Linz, Austria)   (Room C)
Paper
09:50 IN SITU INVESTIGATION OF HYDROGEN ENTRY AND HYDROGEN EMBRITTLEMENT OF ZINC-COATED HIGH STRENGTH STEELS INDUCED BY ATMOSPHERIC CORROSION - Tomas Prosek (University of Chemistry and Technology Prague)   (Room C)
Paper
08:30
Pot Optimization by Numerical Simulation and Material Development - Ari Peltola (SSAB) (until 10:10) (Room B)
08:30 FLOW PATTERN ANALYSIS INSIDE AN IMMERSING SNOUT WITH A PARAMETIC SIMULATION MODEL - Harald Unger (voestalpine Stahl GmbH)   (Room B)
Paper
08:50 SNOUT TEMPERATURE PREDICTIVE MODEL AND Zn POT THERMAL BALANCE - Weimin Zhong (ArcelorMittal Dofasco)   (Room B)
Paper
09:10 Zn VAPOUR INDUCED CORROSION OF 253 MA STAINLESS STEEL END PLATE AND FLANGE IN RETRACTABLE SNOUTS - Daniel Parker (BlueScope Steel Innovation Labs)   (Room B)
Paper
09:50 THE MODIFICATION PROCESS OF THE DROSS BUILD-UP STRUCTURE ON SUBMERGED HARDWARE IN Zn-Al AND Zn-Al-Mg BATHS - Mark Bright (Tata Steel Europe)   (Room B)
Paper
10:10 --- Break ---
10:40
Fundamentals on Absorption of Hydrogen & Fundamentals on Atmospheric Corrosion and Corrosion Modelling -Dr Neil Gao (Senior Research Engineer) Dr Nathalie LeBozec (until 12:20) (Room C)
10:40 RELATIONSHIP BETWEEN HYDROGEN ABSORPTION AND CORROSION BEHAVIOR OF ELECTROGALVANIZED STEEL SHEETS IN DRY-WET CORROSION ENVIRONMENT - Kentaro Hata (JFE Steel Corporation)   (Room C)
Paper
11:00 RECENT ADVANCE IN CORROSION MONITORING OF ATMOSPHERIC CORROSION OF GALVANISED STEEL AND ZINC ALLOYED COATED STEEL - Dominique Thierry (French Corrosion Institute)   (Room C)
Paper
11:20 APPLICATION OF DATA SCIENCE TO ATMOSPHERIC CORROSION PREDICTION - Masataka Omoda (JFE Steel Corporation)   (Room C)
Paper
11:40 ANALYSIS OF COSMETIC CORROSION BEHAVIOR BY IN-SITU OBSERVATION IN WET AND DRY CONDITIONS - Shunsuke Yamamoto (JFE Steel Corporation)   (Room C)
12:00 ATMOSPHERIC CORROSION BEHAVIOURS OF AUTOMOTIVE STEEL SHEETS EXPOSED IN EAST AND SOUTH-EAST ASIA REGIONS - Rinta Sato (JFE Steel Corporation)   (Room C)
Paper
10:40
Fundamentals on Surface Oxidation and Metallic Reactions -Mr Maxime Monnoyer Mr Johann Strutzenberger (until 12:20) (Room A)
10:40 GALVANIZING OF TRIP-Si STEELS - Louis Bordignon (CRM group)   (Room A)
Paper
11:00 EFFECT OF PROCESS ATMOSPHERE DEW POINT AND MINOR Sn ADDITION ON THE SELECTIVE OXIDATION DURING INTERCRITICAL ANNEALING OF A MEDIUM-Mn THIRD GENERATION ADVANCED HIGH STRENGTH STEEL - Kazi Mahmudul Haque Bhadhon (Centre for Automotive Materials and Corrosion, McMaster University)   (Room A)
Paper
11:20 UNDERSTANDING THE EVOLUTION OF SURFACE OXIDES UPON DUAL PHASE STEELS DURING AN ANNEALING CYCLE - Jennifer Rolls (WMG, University of Warwick)   (Room A)
Paper
11:40 UNIQUE SIMULTANEOUS RAPID COOLING AND ZINC COATING TECHNOLOGY - NO BAINITE BEFORE ZINC POT - Pertti Sippola (Psitec Oy)   (Room A)
12:00 ENHANCEMENT OF HOT DIP GALVANIZING ON AS-CAST HIGH-Mn STEEL BY FABRICATION OF FUNCTIONALLY GRADED MULTILAYERS THROUGH LASER CLADDING OF LOW CARBON STEEL - Prof. Jung-Wook Cho (Pohang University of Science and Technology)   (Room A)
Paper
10:40
HDG Bath Hardware -Mr Takashi OKE (until 12:20) (Room B)
10:40 A SIMPLE MODEL TO ESTIMATE AND TRACK THE WEAR RATE OF POT BEARINGS - Michel Dubois (John Cockerill)   (Room B)
Paper
11:00 OFFLINE SIMULATION OF GALVANISING BATH JOURNAL BEARINGS AS A COST EFFECTIVE SOLUTION TO IMPROVE LINE PERFORMANCE AND MITIGATE RISK - Rhys Faulkner (Swansea University)   (Room B)
Paper
PM
12:30 --- Break ---
14:00
Automotive Applications - Zn and ZnFe Coatings -Mr Katsuya Hoshino (JFE Steel Corporation) Dr Bekir Salgin (Tata Steel Europe) (until 15:40) (Room A)
14:00 STRESS CORROSION CRACKING OF HOT FORMING STEELS - Dr Carsten Lachmann (Volkswagen Aktiengesellschaft)   (Room A)
Paper
14:20 THE ROLE OF STEEL SHEET AND ITS IMPACT ON AN OUTSTANDING QUALITY PAINT USED FOR AUTOMOTIVE OUTER SKIN - Friedhelm Macherey (thyssenkrupp Steel Europe AG)   (Room A)
Paper
14:40 Next Generation EDT Technology - Chris Childs (Sarclad)   (Room A)
Paper
15:00 THE EFFECT OF BONDING STATE BETWEEN THE GALVANIZED STEEL SHEETS AND THE ADHESIVE ON DETERIORATION BEHAVIOR OF ADHESIVE JOINT - Masumi Koori (Nipponsteel)   (Room A)
Paper
15:20 AN INNOVATIVE GI WITH IMPROVED GALLING AND SURFACE PROPERTIES FOR EXPOSED AUTOMOTIVE APPLICATIONS - Bart van Veldhuizen (Tata Steel Europe)   (Room A)
Paper
14:00
Furnace II - Current Topics from Preoxidation to Galvannealing - Michel Renard (DREVER International S.A.) Hubert Saint Raymond (Arcelormittal) (until 15:40) (Room B)
14:20 SIMULATION OF FLASH PRE-OXIDATION IN AN ANNEALING SIMULATOR - Marga Zuijderwijk (Tata Steel)   (Room B)
Paper
14:40 ArcelorMittal GENT PRODUCES 3rd GEN. AHSS INCL. Q&P ON THE UNIQUE ANNEALING FURNACE FROM ANDRITZ - Martin Hamman (ANDRITZ) Ann De Boeck (ArcelorMittal Belgium)   (Room B)
Paper
15:00 MULTILAYER ANGULAR ROLL MODEL FOR ONLINE CONTINUOUS CONTROL OF GALVANIZING LINES DRIVEN BY FURNACE MATHEMATICAL MODEL - Alexandre Lhoest (Drever International)   (Room B)
Paper
14:00
Steel-Coating Interfacial Layer and Coating Phase Developments - Thomas Mörtlbauer (voestalpine) (until 15:40) (Room C)
14:00 FORMATION SEQUENCE OF Fe-Al INTERMETALLIC PHASES IN HOT-DIP Zn-Al-Mg ALLOY GALVANIZED STEELS - Naoki Takata (Nagoya University)   (Room C)
Paper
14:20 QUANTITATIVE EVALUATION OF NANOSCALE MECHANICAL PROPERTIES OF Zn-Al AND Zn-Al-Mg COATINGS ON STEEL SHEET BY NANOINDENTATION - Franck Nozahic (ArcelorMittal Global R&D Ghent)   (Room C)
Paper
14:40 IN-SITU OBSERVATION OF THE CRYSTALLIZATION AND GROWTH BEHAVIOR OF Fe-Zn INTERMETALLIC COMPOUND ("BOTTOM DROSS") IN THE MOLTEN ZINC USING X-RAY TRANSMISSION IMAGING METHOD - Ryo Sasaki (kobe steel, ltd.)   (Room C)
Paper
15:00 STRUCTURAL AND MECHANICAL CHARACTERIZATIONS OF TOP DROSS IN A MOLTEN ZINC BATH - Takeshi Konishi (Nippon Steel)   (Room C)
Paper
15:20 INVESTIGATION OF ORANGE PEEL DEFECT ON GALVANIZED DP STEEL SHEET - Lei Cui (Maanshan Iron & Steel Company Ltd,)   (Room C)
Paper
15:40 --- Break ---
16:10
Furnace III - Rapid Cooling, Furnace Roll Coatings - Juliana GUIMARÃES Dr Gerhard Angeli (until 17:30) (Room B)
16:10 EXPERIMENTAL AND NUMERICAL STUDY OF GAS JET COOLING AT HIGH REYNOLDS NUMBER - Mr MICHEL DUBOIS (CMI INDUSTRY)   (Room B)
Paper
16:30 INVESTIGATION OF "BUILD-UP" GROWTH BEHAVIOUR ON HEARTH ROLLS OF CONTINUOUS GALVANIZING LINE - Sho Katsura (KOBE STEEL, LTD)   (Room B)
Paper
16:50 NON STICKING FURNACE ROLLS FOR STEEL PRODUCTS TO IMPROVE SERVICE LIFE AND PRODUCT QUALITY IN CONTINUOUS ANNEALING AND GALVANIZING LINES: PRELIMINARY STUDY ON CHEMICAL INTERACTIONS AND PICKUP MECHANISM - Nicoletta Zacchetti (RINA-Centro Sviluppo Materiali SpA)   (Room B)
Paper
17:10 DEVELOPMENT OF AN ADVANCED ULTRA-FAST COOLING SECTION - Maximilian Schleupen (Department for Industrial Furnaces and Heat Engineering, RWTH Aachen University)   (Room B)
Paper
16:10
Future Aspects of Automotive and Steel Industry - Nathalie Ruscassier John Speer (until 17:30) (Room A)
16:10 AUTOMOTIVE INDUSTRY – QUO VADIS - Prof. Michael Rupp   (Room A)
Paper
16:30 WAYS TO REDUCE CO2 EMISSIONS IN IRON AND STEELMAKING IN EUROPE - Hans-Bodo Lüngen (Executive Member of the Managing Board, VDEh)   (Room A)
Paper
16:10
Non-Automotive Applications: ZnAlMg Coatings and in-line Pre-painted Electrogalvanized Steel -Prof. Joseph McDermid (McMaster University) Dr MOON HONG (POSCO C&C) (until 17:30) (Room C)
16:10 MECHANICAL PROPERTIES AND CRACKING BEHAVIOR OF HOT-DIP GALVANIZED ZnAlMg COATINGS - Masoud Ahmadi (Department of Advanced Production Engineering, University of Groningen)   (Room C)
Paper
16:30 DEVELOPMENT OF ADVANCED PRE-PAINTED Zn-11%Al-3Mg-0.2%Si COATED STEEL SHEETS - Taihei Kaneto (Nippon Steel Corporation)   (Room C)
Paper
16:50 DEVELOPMENT OF ONE LAYER PRE-PAINTED STEEL SHEET - Kunihiko Toshin (NIPPON STEEL CORPORATION)   (Room C)
Paper
17:30
Poster Session (until 18:11) ()
17:30 INFLUENCE OF INTERCRITICAL ANNEALING CYCLES ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF DP980 ADVANCED HIGH-STRENGTH STEEL - Dr Paul R. Provencher (Polytechnique Montreal)   ()
17:32 THE PROPOSAL FOR IMPROVEMENT OF INTERSTITIAL FREE STEEL MECHANICAL PROPERTIES IN CGL PROCESS - Yuki Takeda (JFE Steel)   ()
Paper
17:34 EFFECT OF THE ATMOSPHERE DEW POINT OF CONTINUOUS ANNEALING FURNACES ON THE QUALITY OF GA COATING ON BAKE HARDENING STEEL - Juliana Porto Guimarães (Usiminas)   ()
Paper
17:36 Study on Corrosion Resistance and Adhesion of Paint Coated Zn-Al-Mg Galvanized Steel - Ms Se-Young Oh (POMIA (Pohang Institute of Metal Industry Advancement))   ()
17:38 DEVELOPMENT OF NEW Al COATED STEEL WITHOUT LME CRACKS AND EXCELLENT CORROSION - Suk Kyu Lee (POSCO Technical Research Lab.)   ()
Paper
17:40 KINETICS OF WÜSTITE FORMATION IN SHORT TIME ON PURE IRON IN THE GAS MIXTURE OF CO2+CO OR H2O+H2 - Soroush Aghaeian (Department of Materials Science and Engineering, Delft University of Technology)   ()
Paper
17:42 NEW INDUSTRIAL ACRYLIC RESIN COIL-COATING BOTH ON MECHANICALLY PATTERNED GI AND STS SHEETS - Moon Hi Hong (POSCO C&C)   ()
17:44 INFLUENCE OF DROSS BUILD-UP INDUCED ROUGHNESS ON FLOW STRUCTURES AND HEAT-TRANSFER OF SINK ROLLS IN HOT-DIP GALVANIZING LINES - Georg Reiss (Materials Center Leoben)   ()
17:46 NEW ZnAlMg ALLOY COATINGS WITH ULTRA HIGH CORROSION RESISTANCE - HEUNG YUN KIM (POSCO / Technical Research Laboratories)   ()
Paper
17:48 AN OPTIMIZATION OF SPANGLE MINIMIZER FOR Al-Si COATED STEEL SPANGLE CONTROL - Jong Beom Lee (HYUNDAI STEEL)   ()
17:50 FAST AND NON-DESTRUCTIVE METHOD FOR PHASE QUANTIFICATION IN ZINC ALLOYED COATED STEEL SHEET - Hugues Guerault (Bruker AXS, GmbH)   ()
Poster
17:52 HOW MODEL PREDICTIVE CONTROL ENHANCES STRIP TEMPERATURE REGULATION - Thierry Robin (Fivesgroup)   ()
17:54 EFFECT OF Al CONTENT ON THE CORROSION BEHAVIOR IN Mg-Zn-Al ALLOY COATED STEEL SHEET - Bora Park (POMIA (Pohang Institute of Metal Industry Advancement))   ()
17:56 THROUGH-PROCESS QUALITY CONTROL (TPQC) SYSTEM - ANY DATA, ANY TIME - Can Ergun (Primetals Technologies Austria GmbH)   ()
17:58 SCHEDULING SOLUTIONS SUPPORT SUSTAINABLE PRODUCT QUALITY OF GALVANIZED COILS BY PROVIDING PRODUCTION SCHEDULES IN REPEATABLE QUALITY - Markus Ringhofer (Primetals Technologies Austria)   ()
18:00 SIMULATION AND OPTIMISATION OF A WIPING KNIFE ON THE LAB SCALE - Tobias Klinkberg (Salzgitter Mannesmann Forschung)   ()
Paper
Poster
18:02 NUMERICAL SIMULATION OF BUILD-UP GROWTH COUPLED WITH HYDRODYNAMICS - Georg Reiss (MCL)   ()
Paper
18:04 IN-LINE SEAM WELD INSPECTION USING LASER-ULTRASONICS: RESULTS FROM AN INDUSTRIAL TRIAL - Mr Alexandre Nadeau (Tecnar Automation Ltee)   ()
12:20 --- Break ---
14:00
Fundamentals on Selective Oxidation of AHSS -Prof. Marie-Laurence Giorgi (CentraleSupélec) (until 15:40) (Room C)
14:40 SELECTIVE OXIDATION OF Fe-Mn (1WT.%) BINARY ALLOY DURING CONTINUOUS ANNEALING - Nathalie Ruscassier (Laboratoire LGPM - CentraleSupélec - Université Paris-Saclay)   (Room C)
Paper
15:00 SELECTIVE OXIDATION IN A BAKE HARDENING STEEL FOR DFF - RTF ANNEALING CYCLES - Roel Mallens (TATA steel Research & Development)   (Room C)
14:00
On-Line Measurements and Galvanizing Bath Control Development & Bath Al Chemistry Effects on Coating Quality and Bath Management -Prof. Qi-Fu Zhang (China Iron & Steel Research Institute Group) Dr alessandro ferraiuolo (Marcegaglia Ravenna) (until 15:40) (Room B)
14:00 AN INTEGRATED METHODOLOGY FOR THE ROOT CAUSE ANALYSIS OF MECHANICAL AND METALLURGICAL DEFECTS OF HOT-DIP GALVANIZED COATINGS - Walter DAL'MAZ SILVA (ArcelorMittal)   (Room B)
Paper
14:20 INSPECTING SURFACE QUALITY OF GALVANIZED STEEL BY DEEP LEARNING - Mr Selim Arikan (Smart Steel Technologies)   (Room B)
Paper
14:40 IN-LINE BATH CHEMISTRY MONITORING: REVOLUTIONARY RELIABILITY OF THE NEW DIODE-BASED LASER INDUSTRIAL LIBS SENSOR - Alexandre Nadeau (Tecnar Automation Ltee)   (Room B)
15:00 CELES ECOTRANSFLUX™, A DISRUPTIVE TECHNOLOGY FOR HEATING GEN3 AHSS - Kevin Bertermann   (Room B)
14:00
Physical Vapour Deposition -Mr Yuki Suzuki (NIPPON STEEL CORPORATION / TECHNICAL RESEARCH & DEVELOPMENT BUREAU) Dr Bernd Schuhmacher (thyssenkrupp Steel Europe AG) (until 15:40) (Room A)
14:20 JET VAPOUR DEPOSITION: A TECHNICAL ECONOMIC ALTERNATIVE TO ELECTRO-GALVANIZING FOR Zn COATINGS OF FUTURE STEELS - Daniel CHALEIX (ArcelorMittal)   (Room A)
Paper
14:40 FEEDING TECHNOLOGY FOR A CONTINUOUS PVD COATING LINE - Edzo Zoestbergen (Tata Steel, IJmuiden)   (Room A)
15:00 MECHANISMS STABILIZING GENERAL VAPOUR-PHASE GALVANIZING - Etienne Petit (LEM3 - Université de Lorraine)   (Room A)
Paper
15:40 --- Break ---
16:10
Challenges Galvanizing 2nd and 3rd Generation AHSS - Jean-Michel Mataigne (Arcelormittal) Dr Akihiro Sengoku (until 17:50) (Room A)
16:10 CHALLENGINGS IN GALVANNEALING AHSS AT AN INDUSTRIAL HOT DIP GALVANIZING LINE - Frances Bleich (ArcelorMittal USA)   (Room A)
16:30 U. S. STEEL XG3 – 3rd GENERATION STEEL: CUSTOMER-FRIENDLY CHEMISTRY, PROPERTIES, AND MANUFACTURABILITY ENABLED BY UNIQUE PROCESSING - Matthew McCosby (United States Steel Corporation)   (Room A)
Paper
16:50 EFFECT OF STEEL SUB-SURFACE STRUCTURE ON MECHANICAL PROPERTIES OF GALVANIZED 3rd GENERATION ADVANCED HIGH STRENGTH STEELS - Anirban Chakraborty (ArcelorMittal)   (Room A)
Paper
17:10 EFFECT OF CGL-COMPATIBLE HEAT TREATMENTS ON THE SELECTIVE OXIDATION OF A 0.15C-6Mn-2Al-1Si THIRD-GENERATION ADVANCED HIGH STRENGTH STEEL - Daniella Pallisco (Centre for Automotive Materials and Corrosion, McMaster University)   (Room A)
Paper
16:10
Electrogalvanizing - Process and Product Developments -Dr Edzo Zoestbergen (Tata Steel) Thomas Steck (until 17:50) (Room C)
16:10 INFLUENCE OF ELECTROLYTE COMPOSITION AND TEMPERATURE ON ENERGY DEMAND AND ZINC STRUCTURE DURING ELECTRO-GALVANIZING - Marc Debeaux (Salzgitter Mannesmann Forschung GmbH)   (Room C)
Paper
16:30 EFFECT OF THIOGLYCOLIC ACID ON THE MORPHOLOGY OF Zn ELECTRODEPOSITED ON STEEL SHEETS - Kazuaki Tsuchimoto (JFE Steel Corporation)   (Room C)
Paper
16:50 PREDICTION OF ANODE LIFE TIME IN ELECTRO GALVANIZING LINES BY BIG DATA ANALYSIS - Mario Lovric (Know-Center)   (Room C)
Paper
17:10 IMPACT OF SURFACE TOPOGRAPHY OF ELECTRO GALVANIZED STEEL SHEET ON PAINT APPEARANCE - Johann Gerdenitsch (voestalpine Stahl GmbH)   (Room C)
Paper
16:10
HDG Coating Formation & Dross Management - Sarah Zhang Alexander Mertke (Boliden Commercial Deutschland GmbH) (until 17:50) (Room B)
16:10 INFLUENCE OF Al CONTENT IN THE ZN BATH ON GALVANIZED COATING FORMATION OF HIGH STRENGTH STEELS - Henrique Eleuterio (Usiminas)   (Room B)
Paper
16:30 OPTIMAL CONTENT OF ALUMINUM IN ALUMINUM-ZINC ALLOY IN HOT-DIP COATING ON THE STEEL STRIP - Sergey Yashchuk (JSC Severstal Management)   (Room B)
16:50 A MODELING FRAMEWORK FOR TOP SKIMMING FORMATION IN GALVANIZING BATH - Kintak Raymond Yu (National Research Council Canada)   (Room B)
Paper
17:10 CFD-DPM MODELLING AND ANALYSIS OF DROSS PARTICLE DYNAMICS IN HOT-DIP GALVANIZING BATHS - Werner Eßl (Materials Center Leoben Forschung GmbH)   (Room B)
Paper
17:30 HDG POT PRODUCTIVITY - Matthieu Didier (ArcelorMittal)   (Room B)
Paper
12:20 --- Break ---
14:00
Coating Alloy and Modification effects on Corrosion Behaviour -Mr dominique thierry (French corrosion institute) Dr Vaclav Sefl (until 15:40) (Room C)
14:20 STUDY OF MANGANESE ADDITION ON THE CORROSION RESISTANCE OF GALVANIZED ZINC COATING - Srinivasulu Grandhi (Ph. D Research Scholar)   (Room C)
Paper
14:40 CATASTROPHIC BEHAVIOR OF GALVANIZED STEEL EXPLAINED BY FUNDAMENTALS OF CORROSION SCIENCE - Carlos Arroyave (Arroyave Consulting)   (Room C)
Paper
15:00 THE EFFECT OF PHOSPHORIC ACID ADDED TO CHEMICAL CONVERSION COATING LAYER ON CORROSION PROTECTION IN SCRIBED AREAS OF ZINC-COATED STEELS - Yuki Suzuki (NIPPON STEEL CORPORATION)   (Room C)
Paper
14:00
HDG Coating Weight Control by Nozzle Design & Settings -Mr Jaap van Eenennaam (Tata Steel Europe Research&Development) Owen Pearcy (until 15:40) (Room B)
14:00 PRODUCTION OF HEAVY COATING AT LOW SPEED - MICHEL DUBOIS (CMI INDUSTRY)   (Room B)
Paper
14:20 A NOVEL MULTI-SLOT AIR-KNIFE DESIGN FOR LIGHTER MORE CONSISTENT COATING WEIGHTS IN THE GAS JET WIPING PROCESS - Joseph McDermid (McMaster University)   (Room B)
Paper
14:40 EFFECT OF INITIAL VELOCITY DISTRIBUTIONS IN THE TRANSITION REGION IMPINGEMENT OF SLOT-JET - Gentaro Takeda (JFE Steel Corporation)   (Room B)
15:00 WIPING PRESSURE DYNAMICS AND THEIR EFFECTS ON GALVANIZING COATING SMOOTHNESS - Le Quang Phan (University of Wollongong)   (Room B)
Paper
15:20 WIPING PILOT USE FOR BAFFLE DESIGNS AND SETUP IMPROVEMENTS - Remi Valentin (ArcelorMittal Global R&D)   (Room B)
Paper
14:00
PHS-ZnFe: Liquid and Vapour Metal Induced Embrittlement -Dr Friedrich Luther (Salzgitter Mannesmann Forschung GmbH) Dr Weimin Zhong (ArcelorMittal Dofasco) (until 15:40) (Room A)
14:00 AVOIDING ZINC INDUCED CRACKING IN HOT FORMING - Josef Faderl (voestalpine Stahl GmbH)   (Room A)
Paper
14:20 THE EFFECT OF Si ADDITION ON Zn-ASSISTED LIQUID METAL EMBRITTLEMENT IN 22MnB5 PRESS HARDENING STEEL - Seok-Hyun Hong (Graduate Institute of Ferrous Technology, POSTECH, Pohang 37673, S. Korea)   (Room A)
Paper
14:40 SCANNING ELECTRON MICROSCOPE INVESTIGATION ON ZINC INDUCED CRACKS OF COATED PRESS HARDENED COMPONENTS - Prof. Thomas Antretter (Montanuniversitaet Leoben / Institute of Mechanics)   (Room A)
Paper
15:00 ON THE ORIGIN OF MICRO-CRACKING IN ZINC COATED PRESS HARDENED STEELS - Dr Joseph McDermid   (Room A)
15:20 DEVELOPMENT OF A Zn-Al-Mn-Sb ALLOY COATING FOR PRESS HARDENABLE STEELS - Weiping Sun (Nucor Corporation) Neil Gao (Teck Metals Ltd.)   (Room A)
Paper
15:40 --- Break ---
16:10
Coating Alloy Corrosion Studies - Martin Fieweger (AMEPA - Angewandte Messtechnik & Prozessautomatisierung GmbH) Dr Nega Setargew (BlueScope Steel, Innovation Labs) (until 17:50) (Room C)
16:10 INFLUENCE OF MINOR ADDITION OF Si AND Ti ON THE CORROSION PERFORMANCE OF ZM COATED STEEL - Dominique Thierry (French Corrosion Institute)   (Room C)
Paper
16:30 ELECTROCHEMICAL BEHAVIOR OF Si PHASES IN NOVEL ZnAlMgSi COATINGS - Vaclav Sefl (University of Chemistry and Technology in Prague)   (Room C)
Paper
16:50 THE EFFECT OF MICROSTRUCTURE ON THE CORROSION STABILITY OF ZINC ALUMINIUM MAGNESIUM ALLOYED COATED STEEL IN ATMOSPHERIC CONDITIONS - Nathalie LeBozec (French Corrosion Institute)   (Room C)
Paper
17:10 ZnAlMg METALLIC COATINGS IN HARSH ENVIRONMENTS: A COMPARATIVE AND CHALLENGING STUDY - Philippe Verpoort (ArcelorMittal Global R&D)   (Room C)
Paper
17:30 CORROSION EVALUATION OF THIN Zn-Al ALLOY COATINGS IN A SEVERE MARINE ENVIRONMENT - Neil Gao (Teck Metals Ltd.)   (Room C)
Paper
16:10
HDG Coating Weight Control by Innovative Technological Concepts -Mr MICHEL DUBOIS (CMI INDUSTRY) Mr MinSuh Park (until 17:50) (Room B)
16:10 THE EVOLUTION OF COATING CONTROL SYSTEMS AS THE NEED FOR NEW COATED PRODUCTS EXPANDS - Owen Pearcey (Hatch Ltd)   (Room B)
Paper
16:30 POT ROLL GEOMETRY AND CROSSBOW CORRECTION - MICHEL DUBOIS (CMI INDUSTRY)   (Room B)
Paper
16:50 THE BEHAVIOR OF LIQUID ZINC FLOW IN FULL SPLASHING - Takashi OKE (NIPPON STEEL)   (Room B)
Paper
17:10 EASY ANALYSIS OF AIR KNIFE PERFORMANCE BY STATIONARY FLOW CALCULATIONS - Jaap van Eenennaam (Tata Steel in Europe)   (Room B)
Paper
17:30 ONLINE PHASE FRACTION MEASUREMENT IN A CONTINUOUS ANNEALING FURNACE WITH X-CAP® TECHNOLOGY - Horst Krauthäuser (IMS Messsysteme GmbH)   (Room B)
Paper
16:10
PHS-ZnFe: New Steel & Coating Developments -Dr Thomas Koll (until 17:30) (Room A)
16:30 DEVELOPMENT OF NEW GRADES OF Zn-COATED PRESS-HARDENABLE STEEL COMPATIBLE WITH THE CONTINUOUS GALVANIZING LINE - Chris Thomsen (McMaster University)   (Room A)
Paper
16:50 NANOSCALE INVESTIGATION OF GRAIN BOUNDARY WETTING AND MICRO CRACKS OF PRESS HARDENED GALVANIZED 20MnB8 STEEL - Martin Arndt (voestalpine Stahl GmbH)   (Room A)
Paper
17:10 THE MECHANICAL PROPERTIES AND CRYSTAL STRUCTURE OF Fe-Zn SOLID-SOLUTION IN HOT-STAMPED GA COATING - Akihiro Sengoku (Nagoya R & D Lab., Nippon Steel Corporation)   (Room A)
Paper
17:50
Final remarks (Goodwin, Faderl) (until 18:00) ()